Organic compounds – Test method – Analysis by infrared spectroscopy
Data Sheet by ASD-STAN Standardization, 11/30/1995
ASD-STAN prEN 3462
Titanium alloy TI-P19001 – Annealed – Bar for machining – D <or= 150 mm
Data Sheet by ASD-STAN Standardization, 04/29/1994
ASD-STAN prEN 6059-202
Electrical cables, installation – Protection sleeves – Test methods – Part 202: Dimensions and mass
Data Sheet by ASD-STAN Standardization, 09/30/1997
ASD-STAN prEN 3495
Titanium alloy TI-P19001- Grade 2 – Annealed – Forgings – De <or= 150 mm
Data Sheet by ASD-STAN Standardization, 09/30/1995
ASD-STAN prEN 4612-003
Aerospace series – Cables, electrical, for general purpose, single and multicore assembly XLETFE Family jacketed or screened and jacketed – Part 003: Tin plated copper – Operating temperatures, between – 65 deg C and 135 deg C – Single extruded wall for open a
Data Sheet by ASD-STAN Standardization, 03/31/2005
ASD-STAN prEN 6044-001
Carbon fibre reinforced epoxy prepreg – Technical specification – Part 1 : General requirements
Data Sheet by ASD-STAN Standardization, 12/15/1995
ASD-STAN prEN 6043
Thermosetting resin systems – Test method – Determination of gel time and viscosity
Data Sheet by ASD-STAN Standardization, 11/30/1995
ASD-STAN prEN 4094
Heat resisting alloy – NI-CH1305 (NiCr16Co10Mo8Al4Ti4) – Vacuum melted – Non heat treated – Remelting stock
Data Sheet by ASD-STAN Standardization, 12/31/1997
ASD-STAN prEN 3466
Titanium alloy TI-P63001 – Solution treated and aged– Bar for machining – D <or= 150 mm
Data Sheet by ASD-STAN Standardization, 03/31/1994
ASD-STAN prEN 4090
Steel FE-PL5101 (13MoCrNiV4-4-3-1) – Vacuum induction melted and vacuum arc remelted – Carburized, hardened,sub-zero treated and tempered – Forgings – De <or= 30 mm — 1 315 MPa <or= Rm <or= 1 650 MPa
Data Sheet by ASD-STAN Standardization, 11/28/1997